Last updated: November 2026
Quick answer: Choose the ink system by substrate, press and end use. Water-based flexo ink is strong on absorbent paper, board and corrugated, and dries when its water evaporates or is absorbed. On film it needs a treated surface, a wetting agent and enough drying capacity. Solvent-based ink, in flexo mostly alcohol-based, wets most films and is easy to clean, but its emissions must be controlled. Changing the system also changes treatment, drying, cleaning and the plate grade.
Key takeaways
- Solvent-based flexo ink, in flexo mostly alcohol-based, dries when its solvent evaporates. Water-based ink dries when its water evaporates or is absorbed by the substrate.
- Water-based ink is strong on absorbent paper, board and corrugated. On film it needs a treated surface, a wetting agent and enough drying capacity.
- Alcohol-based ink wets most substrates and is easy to clean, but its solvent emissions have to be controlled.
- Changing the ink system changes the process too: surface treatment, drying, speed, tension, cleaning and the plate grade.
- Start from the end use. The ink supplier and the customer’s specification decide resistance and food-contact questions.
The customer wants water-based ink on film. A new market asks for lower emissions. Or a new substrate arrives and nobody is sure your ink will hold on it. Choosing between solvent based flexo ink and water-based ink depends on the substrate, the press and the end use. This guide compares the two flexo ink types and ends with a decision table.
How solvent-based and water-based flexo inks dry
Both systems have the same four parts: a carrier (solvent or water), a resin that binds the colour to the substrate, a colourant, and additives such as wax. The carrier decides how the ink dries. Our flexographic printing process guide shows where drying fits on the press.
- Solvent-based (alcohol-based) flexo ink. The solvent is mostly alcohol, such as ethanol or n-propanol, often blended with an acetate. Common resins are polyamide and nitrocellulose. The ink dries when the solvent evaporates. Its surface tension is low, so it wets most papers and films well.
- Water-based flexo ink. The resin is usually an acrylic that stays dissolved only while the ink is alkaline, and an amine holds it there; see our water-based flexo ink pH guide. The ink dries when the water evaporates or is absorbed. Water needs more heat to evaporate than alcohol, and humid air slows it further.
Water-based resins differ. A solution resin prints well and redissolves easily, but dries slowly. An emulsion carries more solids and dries faster, but once dry it does not redissolve well.
UV ink is the third system: it cures under UV lamps and does not dry. It has one row in the decision table; our UV flexo ink guide covers it in full.
Choosing flexo ink by substrate
Ink wets a surface only when its surface tension is lower than that of the substrate. Water has a much higher surface tension than untreated polyethylene or polypropylene film.
| Substrate | Water-based ink | Solvent-based ink | Check first |
|---|---|---|---|
| Paper and board | Strong; part of the ink is absorbed, so less drying is needed | Also used | Absorbency; too much solvent or wetting can soften a coating |
| Corrugated board | The usual choice; high-speed work can often run without a dryer | Less usual on absorbent board | Board quality and curl; see corrugated printing |
| PE and PP film | Needs a treated surface, a wetting agent and drying by evaporation only | Wets film well, but the film still needs treatment | Dyne level of every roll |
| PET film | Only on a surface treatment made for it | Suits some treatment types | Which surface treatment the film has; plain film needs a primer |
| Foil and metallised laminates | Choose by the film surface you print on | Which layer carries the print | |
| Film label facestocks | Only on a coated or treated facestock | Uncoated PVC takes alcohol-based or UV ink; uncoated PET takes alcohol-based ink | Whether the facestock has a print coating |
On many metallised laminates the metal sits in the middle, so the ink goes onto a plain film surface. Choose the ink for that film. For film work, see flexible packaging and our dyne level test guide. Water-based inks usually need a higher dyne level than solvent-based inks; the ink supplier gives the value.
Print quality, speed and drying capacity
A common belief is that water-based ink is always the easier choice, because there is less solvent to control. On absorbent paper and board it often is. On film, water-based ink needs a treated surface, enough drying capacity and pH control, and pH is as demanding to control as the solvent balance of an alcohol-based ink.
Drying depends on time (dryer length at a given speed), temperature and air flow.
- Water-based ink on film dries by evaporation only. It needs high temperature, low humidity and the maximum air flow; more heat alone is not enough. Dryers usually run a little hotter than for alcohol-based ink. In humid weather the press may have to slow down.
- Alcohol-based ink dries more easily, but in humid weather the alcohol takes up water, the resin dissolves less well and the print gets dirty. Keep the fountain covered.
- Too much heat forms a skin over wet ink, and residual solvent rises instead of falling. Lower the web temperature first, then talk to the ink supplier about the solvent blend.
“Our dryers cannot handle water-based ink” is a fair objection, so measure first: air flow, air direction and the real web temperature, with an infrared thermometer. If the dryers cannot reach what water-based ink needs on that film, solvent-based ink is the safer choice for that press.
Print quality depends more on the anilox roll, the plate and viscosity than on the ink system. Two points differ. Water-based ink can wear a chrome anilox roll, and a ceramic roll suits it better. For solvent-based ink, correct viscosity first; for water-based ink, check pH first and consider the anilox roll before a viscosity change. Our Zahn cup viscosity guide gives the method. Run as fast as stable drying allows.
Press set-up, cleaning and changeover
Many converters think they can change the ink system and keep the press as it is. When you change the ink, you change the converting process too: surface treatment, drying, speed, tension, chill rolls, viscosity control and often the plate grade.
- Pumps. Corrosion resistant for water-based ink, solvent resistant for solvent-based ink.
- Press stops. Keep water-based ink flowing, or clean the anilox roll at once, before ink dries in the cells.
- Anilox cleaning. At least once a day or once a shift, before the ink dries. Agree the cleaner with the ink and anilox suppliers and avoid strong acids and alkalis. A mild alkaline cleaner without ammonia is common for water-based ink, but too much alkali corrodes chrome rolls. Rinse with water.
- Changeover. Clean the anilox roll, pumps and fountain thoroughly before changing between water-based and alcohol-based ink.
The plate. The ink carrier and the press wash must not swell the plate. Choose the plate grade by ink system and confirm it in the grade’s data sheet; our flexo ink and plate compatibility guide explains the swell test. If you run water-wash flexo plates with solvent-based ink, check that the grade is made for solvent inks.
Emissions and the workplace
Solvent-based ink releases volatile organic compounds (VOC) as it dries. In sunlight, VOC and nitrogen oxides form ground-level ozone, so many regions limit VOC emissions. The usual ways to lower them are water-based, high-solids or UV inks, or treating the exhaust by solvent recovery or oxidation. Local rules decide what is required.
Water-based ink is not always free of VOC, because it can contain some alcohol or other organic solvent. Compare two inks on the same basis: a figure for the whole product and a figure less water and exempt compounds can differ by more than double.
- Read the safety data sheet of every new ink, solvent and wash, and train the crew first.
- Wear gloves and safety glasses with solvents and inks; keep an eyewash station near solvent work.
- Solvent inks need an ink room with earthing and fire and explosion protection.
- Amine vapour from water-based ink can irritate the eyes and skin.
End-use requirements and cost drivers
Choose the ink from the end use. Know how the pack is stored, whether it sees sunlight, how it is packed, conveyed and stacked (this sets the slip, or coefficient of friction), what the product contains, whether condensation forms and what temperatures the pack meets.
- Reverse printing for lamination. Ink inside a laminate must be low in wax and other additives, because too much wax lowers the surface energy and weakens the bond. It should pass tape adhesion, crinkle adhesion and blocking tests.
- Surface printing. Scuff resistance and gloss matter more.
- Food packaging. Low odour and low residual solvent are common requirements. Food-contact suitability is decided by the ink supplier and the customer’s specification, not by the choice of system.
- Higher heat and solvent resistance. Catalysed two-component inks resist heat and solvents better than inks that only dry by evaporation. They must be mixed, have a limited pot life and need specific curing conditions.
Cost drivers. The price per kilogram says little; judge the cost of the dry ink film on the job. The main drivers are ink film weight (set mainly by the anilox roll), viscosity control, white ink run only to the opacity the job needs, colour strength, and with a doctor blade a lower-volume anilox roll instead of extender. Add drying energy, emission control and cleaning time.
Decision table: choosing a flexo ink system
| Your situation | Usual direction | Check first |
|---|---|---|
| Absorbent paper, board, paper bags, corrugated | Water-based | pH control, absorbency |
| Film that cannot be treated | Not water-based; solvent-based only if the film meets the ink supplier’s dyne level | Dyne level |
| Treated film, strong dryers, request for lower emissions | Water-based is possible | Wetting agent, drying, ceramic anilox, press trial |
| Film with limited drying capacity | Solvent-based | Emission control, residual solvent |
| Reverse printing for lamination | Either, in a low-wax laminating grade | Tape, crinkle and blocking tests |
| Uncoated PVC or PET label facestock | Alcohol-based (PVC also UV), or a coated facestock | Facestock coating |
| High heat or solvent resistance | Catalysed two-component ink | Pot life, curing conditions |
| Ink must not dry on the plate; UV lamps on press | UV ink; see the UV flexo ink guide | Curing unit, plate grade |
“Solvent-based ink is the only thing that works on film” is true for some presses, not all. Where the film is treated and the dryers have the capacity, water-based ink can run on film. Confirm the choice with a press trial on the real substrate, and when the ink comes off the film, check the dyne level and the drying before you blame the ink.
FAQ
What is the difference between solvent-based and water-based flexo ink?
The carrier. Solvent-based ink, mostly alcohol-based in flexo, dries when its solvent evaporates. Water-based ink dries when its water evaporates or is absorbed, and it needs more heat to dry.
What is alcohol-based flexo ink?
The usual form of solvent-based flexo ink. The solvent is mostly alcohol, such as ethanol or n-propanol, often with an acetate. Its low surface tension lets it wet most papers and films.
Can water-based flexo ink be used on plastic film?
Yes, if the film has a treated surface, the ink contains a wetting agent and the dryers give high temperature, low humidity and the maximum air flow.
Which flexo ink is best for corrugated board?
Water-based ink is the usual choice. Absorbent board takes up the ink, and high-speed work can often run without a dryer.
What has to change when you switch from solvent-based to water-based ink?
Surface treatment, drying, speed, tension, chill rolls, viscosity and pH control, pump materials, cleaning and often the plate grade. Clean the anilox roll, pumps and fountain thoroughly first.
Is water-based flexo ink free of VOC?
Not always, because it can contain some alcohol or other organic solvent. Compare VOC figures on the same basis.
Changing ink system? We supply flexo plates. Request a quote with your ink system, press wash, substrate and plate thickness, or ask a technical question.
Disclaimer: this page describes general flexographic pressroom practice and is for reference only. Ink selection, end-use resistance and food-contact suitability are subject to your ink supplier’s data sheets and your customer’s specification; emission limits are subject to local regulations.