Last updated: November 2026
Quick answer: Flexo barring is light and dark bands across the web at a regular spacing. Measure the spacing over several bars and compare it with the gear tooth spacing, the plate cylinder repeat and the anilox circumference. Then check, in order, mounting tape, the pressure and parallelism of the anilox, plate cylinder and impression cylinder, cylinder and sleeve accuracy, and the gears. More impression does not remove the cause.
Key takeaways
- Flexo barring is light and dark bands across the web, at right angles to the direction of travel. Streaks along the web are a different fault.
- Measure the distance between the bars before you change anything. Compare it with the gear tooth spacing, the plate cylinder repeat and the anilox circumference.
- Common press-side causes are a unit not set to its standard, poor plate cylinder accuracy, mounting tape that differs in density, and wrong pressure or parallelism between the anilox, plate cylinder and impression cylinder.
- Gears keep the three cylinders at the same surface speed only when each gear’s pitch diameter matches the diameter it drives.
- More impression does not remove the cause of bars. Set the three cylinders parallel at the lightest pressure that prints.
You see bars across the web at the same spacing. The solids show light and dark bands. The bars come at a certain speed and fade at another, or the solid skips and repeats at the same place in every repeat. Barring, gear marks and plate bounce look alike, but they come from different parts of the press. This guide shows how to tell them apart, how to measure the repeat of the bars and link it to a part of the press, and which fixes to try first.
What barring, gear marks and plate bounce look like
All three show as banding across the web, easiest to see in solids and even tints.
- Barring (bars or banding). Light and dark bands across the web, at right angles to the direction of travel, repeating at a fixed spacing.
- Gear marks. Fine, evenly spaced bands at the same spacing as the teeth of a gear in the drive.
- Plate bounce. A bar, or a short area where the solid skips and then prints again, at the same place in every repeat, often just after the plate gap or the lead edge of a large solid.
Some faults look similar but are not barring:
- Streaks along the web come from a worn doctor blade, a scratched anilox or a damaged plate. Fine streaks in the print direction can also come from low viscosity ink at a heavy ink feed, ink with poor flow, or a coarse anilox screen. See doctor blade streaks.
- Irregular streaks or spots with no regular spacing point to the ink, the substrate or the plate surface.
- Ghosting (double image) comes from too much printing pressure, too much ink, a worn plate or plate cylinder, or tape that is too hard.
- Stripes that follow the flutes on corrugated board are a board fault. See corrugated washboarding.
Measure the repeat before you change anything
A common belief is that barring is an ink or plate problem, so the first move is to change the ink or remake the plate. Measure the repeat of the bars first: the spacing links the bars to a gear, a cylinder or sleeve, or the plate gap. A new plate will not cure a bar that comes from the drive.
Take a length of printed web with several bars. Measure from the centre of one bar to the centre of a bar several bars further on, and divide by the number of spaces. Then note whether the bars show in every colour or in one, and at which press speeds they appear and fade.
| What you measure | Where to look first |
|---|---|
| Bars at the tooth spacing of a drive gear | That gear and the gears it meshes with |
| One bar per plate cylinder turn, same place in every repeat | Plate gap, lead edge of a solid, mounting, tape, plate cylinder or sleeve |
| Bars at the anilox circumference | The anilox roll: runout, damage, its drive |
| Bars in one colour only | That unit: mounting, pressures and cylinders |
| Bars in every colour at the same spacing | Parts shared by all units, such as the main drive |
| Bars that come and go with press speed | Record the speeds; check the drive and bounce at the gap |
| No regular spacing | Not barring: check ink, substrate and plate surface |
Work from the simplest check to the most costly: mounting and tape, then pressure and parallelism, then cylinder, sleeve and anilox accuracy, then the gears and drive. Write the spacing, unit and speed in the shift log. Our guide to print quality control charts shows how to keep press records that show a trend.
Gears and drive: what gear marks tell you
On a geared flexo unit, the plate cylinder, anilox and impression cylinder must run at the same surface speed. The gears do this only when each gear’s pitch diameter matches the surface it drives:
- Plate cylinder: gear pitch diameter equals the outside diameter of the mounted plate, that is the cylinder or sleeve with tape and plate on it.
- Anilox: gear pitch diameter equals the outside diameter of the anilox roll.
- Impression cylinder: gear pitch diameter equals the cylinder diameter plus twice the substrate thickness.
Pitch diameter equals the number of teeth times the circular pitch, divided by 3.1416, and the printed repeat equals the number of teeth times the circular pitch. Presses built to US practice use 1/4 in circular pitch or 10 diametral pitch gears; metric gears are given by module. Confirm which system your press uses and do not mix them.
When the surfaces do not run at the same speed, the plate gets dirty, register suffers and the plate wears faster. Some printers say “the press is new, the gears are fine”. A new press still needs the right mounted diameter for its gear, and a change in plate or tape thickness changes that diameter. See flexo sleeves and mounting tape for how sleeve, tape and plate set the repeat.
Bars at tooth spacing point to worn or damaged teeth, a gear that does not suit the mounted diameter, excess impression or bounce. Keep the press maintained to the press maker’s specification, including gear wear, repeat accuracy, and the runout and parallelism of the anilox and impression rolls. On gearless, servo-driven presses these gear rules do not apply; regular bars there are a matter for the press maker’s service team.
Cylinders, sleeves, anilox and mounting tape
When there is one bar per turn of a cylinder, check that cylinder and what is mounted on it.
- Plate cylinder. A plate cylinder with poor accuracy gives bars. The fix is to replace it.
- Sleeves. Sleeve runout or a damaged sleeve gives bounce and banding. Check that the sleeve runs true.
- Anilox. One published set of conditions for running a doctor blade asks for total anilox runout of no more than 0.0005 in (about 0.013 mm). This is a strict value; the press maker’s or anilox supplier’s data decides. See our anilox roller guide.
- Mounting tape. Tape that differs in density gives bars. Choose tape of high, medium or low density to suit the job; in halftone work, use a resilient, low-density tape.
- Mounting. Check that tape and plate are pressed down evenly, with no trapped air and no lifting edges. Our flexo plate mounting guide gives the steps.
Impression and the three-cylinder setting
Many operators believe more impression will print the bars out. More impression does not remove the cause: set the anilox, plate cylinder and impression cylinder parallel at the lightest pressure that prints. Extra squeeze can hide a bar for a while, but it brings ghosting, dirty fine dots and plate wear.
- Set the unit to its standard. Adjust the connections of each part to the press maker’s standard before you change anything else.
- Parallelism. Set anilox to plate cylinder, and plate cylinder to impression cylinder, parallel across the full width. Uneven pressure at the two ends of the cylinder also gives weak, unclear print.
- Pressure. Set both nips as light as will print a full solid. Too much pressure at either point dirties fine dots.
- Corrugated board. More pressure crushes the flutes and lowers board strength.
Our flexo printing problems guide covers other faults that come from too much impression.
Plate bounce at the gap and the lead edge
Where the plate does not wrap the full circumference, the plate gap passes through the nip once in every turn. A large solid that starts right at the lead edge meets the impression cylinder all at once. Both can make the cylinder jump, and the print shows a bar or skip at the same place in each repeat.
- Where the layout allows, keep the plate gap away from solids, and do not start a large solid right at the lead edge.
- Bevel or seal the plate edges, and press the tape down well at the lead edge.
- For the shock from uneven plate height, one common method is a bearer strip on each side of the plate, wrapping the whole plate cylinder.
- Check that plate thickness and hardness suit the substrate. Our flexo plates page lists the plate types we supply.
Flexo barring troubleshooting table
| Symptom | Likely cause | Check or fix |
|---|---|---|
| Fine bars at gear tooth spacing | Worn or damaged teeth; gear does not match the mounted diameter | Inspect the gears; check plate, tape and sleeve against the gear |
| Regular bars in one unit | Unit not set to its standard; wrong pressure or parallelism of the three cylinders | Reset the unit; set the cylinders parallel at the lightest pressure that prints |
| One bar per plate cylinder turn | Poor plate cylinder accuracy; sleeve runout or damage | Check runout; replace the plate cylinder or sleeve |
| Bars at the anilox circumference | Anilox runout or damage | Check against the supplier’s data; repair or replace the roll |
| Light and dark bands in solids | Mounting tape that differs in density | Choose tape density to suit the job |
| Bar or skip after the plate gap or lead edge | Plate bounce; uneven plate height | Move the gap away from solids; seal edges; fit bearer strips |
FAQ
What causes barring in flexo printing?
Common causes are a unit not set to its standard, poor plate cylinder accuracy, tape that differs in density, and wrong pressure or parallelism of the three cylinders. Gears, runout and plate bounce also give bars.
What are gear marks in flexo printing?
Fine, evenly spaced bands across the web at the tooth spacing of a drive gear. They point to worn or damaged gears, or a gear that does not match the diameter it drives.
How do I find which part of the press causes the bars?
Measure the spacing over several bars and compare it with the gear tooth spacing, the plate cylinder repeat and the anilox circumference. Note which colours show the bars and at which speeds.
What is plate bounce in flexo?
A jump of the plate cylinder when the plate gap or the lead edge of a large solid enters the nip. It shows as a bar or skip at the same place in every repeat.
Will more impression remove bars?
No. It does not remove the cause and brings ghosting, dirty fine dots and plate wear. Set the three cylinders parallel at the lightest pressure that prints.
What is the difference between bars and streaks in flexo?
Bars run across the web and repeat at a fixed spacing. Streaks run along the web and come from a worn doctor blade, a scratched anilox, a damaged plate or the ink.
Plates for a new job or a new press? Request a quote with your press, repeat, plate thickness and substrate, or ask a technical question about the bars you see.
Disclaimer: the causes and checks on this page are general pressroom practice and for reference only. Gear, runout and pressure settings for your press are subject to the press manufacturer’s manual and the supplier’s data sheets.