Quick answer: Ink trapping is how well a printed ink film accepts the next ink printed on top of it, usually wet-on-wet on a multicolour offset press. Poor trap makes reds, greens and blues look weak or dirty. It is measured with a densitometer, and it is controlled mainly by ink tack sequence, ink film thickness, water level and colour sequence.

Key takeaways

  • “Trapping” means two things: ink acceptance on press, and colour overlaps added in prepress. This post is about the press side.
  • Measure apparent trap on overprint patches in the colour bar, not by eye.
  • In wet-on-wet printing, each ink should have lower tack than the ink printed before it.
  • Too much water is one of the most common and least suspected causes of poor trap.

A job can hit every solid density target and still look wrong because the overprints are weak. Red looks orange, green looks thin, dark blue looks purple. Press crews often add more of the second ink, which raises dot gain without fixing the overprint. This guide explains what ink trapping is, how to put a number on it, and which settings actually move it.

What is ink trapping?

On a four-colour press, the second, third and fourth inks are printed onto ink films that are still wet. Ink trapping describes how much of the new ink transfers onto the wet film compared with how much would transfer onto bare paper. Good trap gives clean, saturated overprints. Poor trap means the second ink does not stick well to the first, so the overprint lacks colour.

The opposite fault also exists: back-trapping, where ink already on the sheet is picked back up by the blanket of a later unit. Back-trapping often shows as mottled solids and is covered in our print mottling guide.

Press ink trap vs prepress trapping

Term Where it happens Purpose Who controls it
Ink trap (this post) On press, wet-on-wet One ink film accepting the next Press crew, ink choice, dampening
Prepress trapping (spread / choke) In the RIP or design file Small colour overlaps that hide misregister gaps Prepress operator

Prepress trapping is set in the workflow before the plate is imaged; see our CTP RIP workflow post for where it sits. Neither kind of trapping can replace the other: a good prepress trap will not save an overprint that the press cannot trap.

How to measure ink trap

Most pressrooms use the Preucil formula for apparent trap, read with a densitometer on the colour bar:

Trap % = (Dop − D1) ÷ D2 × 100

  • Dop = density of the overprint patch (for example red, magenta then yellow)
  • D1 = density of the first-down ink solid
  • D2 = density of the second-down ink solid

All three readings are taken through the filter of the second-down ink: for a red made of magenta then yellow, use the blue filter that reads yellow. The result is called “apparent” trap because gloss, ink opacity and paper also affect the reading. Use it to compare sheets, shifts and settings on the same paper, and keep your own target from good reference jobs rather than chasing a number from another plant.

What causes poor ink trapping?

  • Wrong tack sequence. If a later ink is tackier than the film it lands on, it pulls the first ink back instead of sticking to it.
  • Too much water. A layer of fountain solution on the first ink film, or a heavily emulsified ink, keeps the next ink from bonding. See ink and water balance.
  • Unbalanced ink film thickness. A very heavy first-down film with a thin second film is hard to trap over.
  • Colour sequence. Changing the laydown order changes which ink is under which, and so the overprint colour.
  • Paper. Absorbent uncoated stock pulls vehicle out of the first film quickly, which changes trap compared with coated stock.
  • Temperature. Warm rollers lower ink tack, so a sequence that traps well in the morning may not after hours of running.

Ink trapping troubleshooting table

Symptom Likely cause Check / fix
Red looks orange, green looks yellowish Second ink not trapping on the first Read apparent trap; check ink tack sequence with the ink supplier
Trap falls as the run warms up Roller temperature lowering tack Check roller temperature control; note settings when trap is good
Trap poor and fountain tray coloured Too much water, over-emulsified ink Run the lowest stable water; check fountain solution dose and conductivity
Solids mottled in later units Back-trapping onto later blankets Review tack sequence and blanket condition
Overprints differ between operator side and drive side Uneven dampening or ink keys across the plate Check dampening rollers and ink key profile
Plate needs a lot of water to stay clean Plate or platemaking issue raising the water level Check development and gumming; see the plate checks below

How to improve ink trapping on press

  1. Measure first. Read apparent trap for red, green and blue on several sheets before changing anything.
  2. Bring water down to the lowest level that keeps the plate clean. This alone often improves trap.
  3. Confirm the tack sequence with your ink supplier. A common laydown is black, cyan, magenta, yellow, with tack decreasing in that order, but follow the ink set’s data sheet.
  4. Balance the films. Avoid running the first-down ink far above its density target to compensate for something else.
  5. Control temperature of the inking rollers where the press allows it.
  6. Keep the fountain solution in range; the fountain solution guide covers dose, pH and conductivity.
  7. Record the good settings for each paper so the next shift starts from them.

Where the plate fits in

The plate does not set trap directly, but it sets how much water the press needs. A plate with clean, fully developed non-image areas runs at a lower water level, which helps trap. Under-developed or poorly gummed plates push operators to add water. Our thermal CTP plates and CTcP plates come with a grade TDS for developer and processing settings. For UV inks, which cure between units and change how trap behaves, read printing plates for UV ink before choosing a plate: single-layer thermal and CTcP plates are not UV-ink resistant.

FAQ

What is ink trapping in offset printing?

Ink trapping is the ability of a wet ink film on the sheet to accept the next ink printed over it. Good trap gives clean red, green and blue overprints; poor trap makes them weak or shifted in hue.

How do you calculate ink trap?

Use the Preucil formula: trap % = (overprint density minus first-down ink density) divided by second-down ink density, times 100. Take all three readings with a densitometer through the filter of the second-down ink.

What causes poor ink trapping?

The usual causes are a wrong tack sequence, too much water or over-emulsified ink, a heavy first-down ink film, a changed colour sequence, absorbent paper and warm rollers that lower tack.

How does ink tack affect trapping?

In wet-on-wet printing each ink should be less tacky than the ink film it lands on. If a later ink is tackier, it pulls the first ink back onto the blanket instead of sticking to it, which gives poor trap and back-trapping.

What is the difference between ink trapping and prepress trapping?

Ink trapping is the press-side transfer of one wet ink onto another. Prepress trapping adds small colour overlaps (spreads and chokes) in the file or RIP to hide misregister. They solve different problems and one cannot replace the other.

Want a plate that runs clean at low water? Request a quote and send your press size, plate size and gauge, platesetter type and ink system (conventional or UV). Or request trial plates / contact us.

Disclaimer: values on this page are typical and for reference only; final specifications, MOQ, price and lead time are subject to the grade TDS and the quotation.

About Peter Zhang

Peter Zhang is Sales Manager at CTPPress, helping printers and dealers choose CTP plates, flexo plates and prepress equipment. Questions about a plate or machine? Contact us and we will reply with a specific recommendation.

Talk With Author >>

Start Your Business With Us

Simple Contact Form

Tell us what you need

Request a Quote

Tell us which printing plates or equipment you need, including specifications, quantity and destination. Use the form to send your enquiry.

Aluminium coils and printing plate production equipment
Product Enquiry

Request an Instant Quote

We reply within 24 hours on working days

Product Enquiry
Aluminium coil on an offset plate production line

Send an Enquiry


Product Enquiry
Chat on WhatsApp