Last updated: November 2026
Quick answer: An EPDM roller is the usual choice for UV and LED-UV ink, and a nitrile (NBR) roller for conventional oil-based ink. Rubber swells or shrinks in liquids that are chemically similar to it: nitrile resists mineral oil and petroleum washes but is weak in ketones and esters, and EPDM is the opposite. Match the compound to the ink and the wash first, then choose the hardness. A press that runs both ink systems needs a compound tested for mixed use.
Key takeaways
- Rubber swells or shrinks in liquids that are chemically similar to it. The roller compound has to match every liquid that touches it: the ink, the wash and the fountain solution.
- Nitrile (NBR) resists mineral oil and aliphatic (petroleum) washes, so it is the usual rubber for conventional oil-based ink. It is weaker in ketones and esters.
- EPDM resists water, alcohols, ketones and esters, and it is the usual rubber for UV and LED-UV ink. It swells in mineral oil and petroleum washes.
- A mixed-mode press that runs both conventional and UV inks needs a compound tested against both inks and both washes.
- Choose the compound first and the hardness second. Offset ink rollers typically run at about 20 to 40 Shore A.
“Our rollers swelled after we changed to UV ink.” “The rollers have gone soft and sticky.” “The roller ends are cracking and the stripes will not hold.” All three often have the same cause: the rubber on the roller does not suit a liquid that touches it. Before you order a replacement set, you need to know which rubber to order for your ink. This guide compares the two rubbers used most for offset printing rollers: the nitrile roller (NBR) and the EPDM roller.
Why the roller compound has to match the ink and the wash
“Rubber is rubber, only the size matters” is a common belief: any rubber roller of the right size will run any ink. It will not. The rubber compound has to match the ink and the wash, because rubber swells or shrinks in liquids of similar polarity.
Ink contains vegetable oils, mineral oils and sometimes solvents, and the wash is a solvent blend. These liquids can enter the surface layer of the rubber. If the rubber cannot resist them, the roller swells or shrinks, and the roller setting changes with it. A rubber takes up liquids that are chemically similar to it and resists liquids that are different.
- Non-polar liquids: mineral oil and aliphatic (petroleum) solvents.
- Polar liquids: water, alcohols, ketones and esters.
- Nitrile is a polar rubber. It resists non-polar oils.
- EPDM is a non-polar rubber. It resists polar liquids and takes up oil.
A roller swells when the rubber takes up liquid. It shrinks when a liquid removes the plasticisers and softeners that are part of the compound. In one published test, a nitrile roller compound of 30 Shore A was soaked for 24 hours at room temperature. It gained 1.4% in mass in high-boiling kerosene and lost 3.3% in linseed oil. The same rubber moved in opposite directions in two liquids.
What nitrile (NBR) rollers suit
Nitrile is the usual roller rubber for conventional oil-based offset ink.
- Strong points: mineral oil, lubricating oil and aliphatic (petroleum) solvents. Nitrile is also rated well in water and alcohol, and one step above EPDM for abrasion resistance.
- Weak points: ketones (rated fair only), esters such as ethyl acetate (rated poor to fair) and chlorinated solvents (rated poor).
- Not settled: aromatic solvents such as toluene and xylene. Published ratings for this combination disagree, so confirm it with the roller supplier before you use a wash that contains them.
A standard nitrile roller is not suited to UV ink: rollers made for conventional ink swell or shrink when they run UV ink and are cleaned with UV wash.
What EPDM rollers suit
EPDM is the usual rubber for UV ink rollers, on UV and LED-UV presses alike. UV inks are built on reactive monomers and resins, not on drying oils and mineral oil, and they are cleaned with their own UV washes.
- Strong points: water, alcohols, ketones and esters. EPDM is also rated excellent against ozone and ageing.
- Weak points: mineral oil, lubricating oil and aliphatic (petroleum) solvents (all rated poor), aromatic solvents and chlorinated solvents.
“EPDM is the UV rubber, so it must be safe for everything” is the second belief to correct. EPDM is not the better rubber for every press. EPDM suits UV ink and polar washes but swells in the mineral oil of conventional ink; nitrile is the opposite. A petroleum wash can swell an EPDM roller.
There is no general rating for “UV ink” or “UV wash” as a class. The working rule is that every roller in a UV press, the dampening rollers included, has to resist the UV ink and the UV wash that are actually used. Give the data sheets for both to the roller supplier. For UV flexo curing, see UV flexo ink. For the rest of the change to UV, see UV and LED-UV offset and printing plates for UV ink.
NBR vs EPDM rollers: compound against ink and wash type
The table is a first screen for a rubber roller compound. “Good” means rated good or better. Formulations inside one rubber family differ a lot, so the roller supplier’s data sheet decides.
| What touches the roller | Nitrile (NBR) | EPDM |
|---|---|---|
| Mineral oil, lubricating oil, aliphatic (petroleum) solvents and washes | Good | Poor |
| Aromatic solvents (toluene, xylene) | Ratings disagree: confirm with the roller supplier | Poor |
| Chlorinated solvents | Poor | Poor |
| Ketones | Fair | Good |
| Esters (ethyl acetate) | Poor to fair | Good |
| Water and alcohols | Good | Good |
| Ozone | Ratings disagree: confirm with the roller supplier | Good |
| Conventional oil-based ink with a petroleum wash | Usual choice | Not suited |
| UV or LED-UV ink with a UV wash | Not suited | Usual choice |
| Both ink systems on one press | Neither standard compound: ask for a compound tested for mixed use | |
Mixed-mode presses that run conventional and UV inks
Many printers want one set of rollers that runs both conventional and UV ink. A standard compound cannot do this. The UV ink and the UV wash attack a nitrile set, and the conventional ink and the petroleum wash swell an EPDM set.
- Ask for a mixed-mode compound. Roller suppliers offer compounds for presses that change between the two ink systems. Such a compound has to be tested against both inks and both washes, so name all four when you order.
- Choose the washes with the compound. Two different washes meet the same rubber, so use only washes that the roller supplier accepts for it.
- Include the dampening rollers. They meet the same ink and the same wash as the inking rollers.
- Hybrid inks. Ask the ink supplier which roller compound and which wash the ink is made for.
The wash and the fountain solution
It is easy to think that only the ink decides the roller rubber. “The wash only cleans, it cannot damage the roller” is not true: a compound that suits the ink can still swell in the wrong wash. So list every liquid that touches the roller: ink, wash and fountain solution.
- Find the solvent family of the wash. Do not guess it. Ask for the technical data sheet and compare the family with the table above.
- Match the wash to the ink system and the compound. A roller wash for conventional ink goes with nitrile rollers. UV ink needs a UV wash, and the rollers have to resist it.
- Treat deglazers the same way. The roller deglazer guide explains when to use one.
Fountain solution is mostly water and sometimes contains alcohol. Nitrile and EPDM are both rated good or better in water and in alcohol, so the fountain solution does not usually decide between the two rubbers. The ink and the wash do. Dampening rollers must resist the fountain solution, resist ink building up on the surface and keep the water feed stable. On a UV press they must also resist the UV wash, so they follow the same ink system as the inking rollers. For the water side, see the fountain solution guide.
How to recognise roller swelling, shrinking, hardening and cracking
Before you order the same compound again, compare the diameter and the Shore A hardness with the values the roller had when new, and look at the surface.
| Sign | What you see | Likely cause | What to do |
|---|---|---|---|
| Roller swelling | Larger diameter, wider stripe, soft or sticky surface, often worse at the ends | The rubber takes up oil or solvent from the ink or the wash | Compare every liquid with the compound; change the compound or the wash |
| Shrinking | Smaller diameter, narrower stripe | A liquid removes plasticisers from the compound | Check the wash first; reset or replace the roller |
| Hardening | Hardness above the value when new, shiny glazed surface | Age, heat, glaze, loss of plasticisers | Deglaze, then measure the hardness; replace if it stays hard |
| Cracking | Fine cracks on the surface or at the ends | Ozone and ageing, or rubber that has shrunk and hardened | Replace; a cracked roller cannot be recovered by cleaning |
Test a new wash or ink before it goes on the press. Take a piece of the same rubber, weigh it, soak it in the liquid for 24 hours at room temperature, then weigh and measure it again. A clear gain means swelling. A loss means the liquid is removing part of the compound.
Hardness: the second choice after the compound
Hardness comes second because it does not stay correct in the wrong rubber. A roller that swells becomes softer, and a roller that loses plasticiser becomes harder. Rollers that hold their setting start with the right compound.
- Offset ink rollers: typically about 20 to 40 Shore A, with high-speed presses at about 30 to 40 Shore A.
- Offset dampening rollers: typically about 20 to 30 Shore A.
- Too soft: the roller resists chemical attack less well and builds up heat.
- Too hard: the roller transfers ink less well, absorbs less vibration and, over time, wears the precision of the press.
These are typical values, not requirements. There is no fixed speed at which a press counts as high-speed, so the press manual and the roller supplier’s data sheet decide the hardness for each position.
FAQ
What is an EPDM roller used for?
Mainly for presses that run UV or LED-UV ink. EPDM resists water, alcohols, ketones and esters, but it is rated poor in mineral oil and petroleum washes, so it is not suited to conventional oil-based ink.
Can nitrile rollers run UV ink?
Not with a standard compound. Rollers made for conventional ink swell or shrink when they run UV ink and are cleaned with UV wash.
Why do rubber rollers swell?
The rubber takes up a liquid that is chemically similar to it, for example mineral oil in EPDM. The liquid can come from the ink or from the wash, so check both against the compound.
Can one set of rollers run both conventional and UV ink?
Not a standard nitrile or EPDM set. A mixed-mode press needs a compound tested against both inks and both washes. Name all four liquids when you order.
How do I know whether a roller has swollen or shrunk?
Compare the diameter and the Shore A hardness with the values when new. A swollen roller is larger and softer and gives a wider stripe. A shrunk roller is smaller and gives a narrower stripe.
What hardness should offset ink rollers be?
Offset ink rollers typically run at about 20 to 40 Shore A, with high-speed presses at about 30 to 40, and dampening rollers at about 20 to 30 Shore A. The press manual and the roller supplier’s data sheet decide the value for each position.
To order compatible replacement rollers: request a quote and send the press model, the roller position, the ink type and the wash type. See printing rubber rollers for the roller range, or ask a technical question.
Disclaimer: the resistance ratings and hardness ranges on this page are for reference only. Rubber formulations differ, so confirm the compound with the roller supplier and test new inks and washes before use. Hardness for your press is subject to the press manufacturer’s manual.