Quote Now

Anilox Volume Chart: Line Screen and BCM by Job Type

Written by
Feng Yan
Last update:

By Feng Yan, Technical Engineer, CTPPressLast updated: November 2026Quick answer: Anilox BCM is the ink…

By Feng Yan, Technical Engineer, CTPPress

Last updated: November 2026

Quick answer: Anilox BCM is the ink volume the cells hold, in billion cubic microns per square inch. Choose from the job: solids need a coarse screen and high volume, halftones a fine screen and low volume, and absorbent paper more volume than film. For halftones, use an anilox line screen at least four times the plate screen ruling, and five to six times to hold 1 to 3% dots. Confirm the choice with your anilox supplier’s current data and a press trial.

Key takeaways

  • Line screen is the number of cells per inch. Cell volume is the ink the cells hold per area, in BCM per square inch or cm³/m².
  • Aim for the thinnest ink film that still gives full colour strength. Paper needs more volume than film; solids need more volume than dots.
  • For halftones, use an anilox at least four times the plate screen ruling, and five to six times to hold 1 to 3% dots.
  • The volume chart is one supplier’s 1999 data from one measuring method. Check it against your supplier’s current data.
  • A shop volume test will not match the supplier’s figure. Use it to track wear on the same roll.

The highlight dots are dropping out, or they print dirty and heavy. Colour is getting weaker but the ink is the same. A new job arrives and we do not know which anilox to put on for this job. This reference page gives a chart we can start from, the rule that links the anilox to the plate screen, and a way to check anilox BCM and wear on press.

Line screen and cell volume

Line screen is the number of engraved cells per inch, in lpi. A finer screen means smaller cells. Cell volume is the ink the cells hold per area. US data gives it in BCM per square inch (billion cubic microns per square inch), metric data in cm³/m². Check which unit a data sheet uses before you compare two rolls. This page uses BCM per square inch. Our anilox roller guide covers anilox basics and gives the conversion.

Many printers believe that a higher BCM always gives better colour. It does not. The aim in flexo is the thinnest ink film that still gives full colour strength, so volume is matched to the substrate and the print content. A fine, low-volume anilox and a fast-drying ink of high colour strength both help. Too much volume floods small dots; see flexo dot gain.

Line screen and volume are linked: a fine screen has small cells and cannot hold a high volume. Cells with a depth-to-opening ratio of 23 to 33% take up and release ink best. This matters most at 440 lpi and finer. Too deep a cell plugs easily; too shallow a cell is hard to engrave and to reproduce. The anilox supplier sets the engraving.

Start from the job: substrate and print content

First look at the press and the crew: impression range, register accuracy, dot gain, and whether the operators get stable results. Then look at the job:

  • Substrate. Absorbent paper and board need more volume than film or foil.
  • Print content. Solids need high volume and a coarse screen; halftone dots a fine screen and low volume.

Typical starting points for coarse screens:

Print content Absorbent paper: lpi / BCM per in² Film: lpi / BCM per in²
Solids 180 / 9.5 220 / 7.5
Line work and text 200 / 8.3 250 / 7.0
Halftones 250 / 7.0 360 / 4.5

These values apply only to halftone screens of 85 lpi or coarser. Real values depend on the press, its speed, the operator and the substrate surface, so agree them with your ink and anilox suppliers. Published values do not all agree: another example puts solids on wide-web film at 220 lpi and 7.7 BCM; the paper values for solids and line work are above the top of the chart range for 180 and 200 lpi; and 250 lpi for paper halftones is less than four times an 85 lpi screen. Where values differ, the supplier’s data sheet and a trial decide. For finer screens, use the ratio rule below.

For the plate side of each market, see flexible packaging, label printing and corrugated printing.

Anilox volume chart by line screen

Once the line screen is chosen, read its volume range. The table shows selected rows from one supplier’s published figures from 1999, measured by vertical scanning interferometry. Another method can give different values, and engraving has changed since then, so check every row against your anilox supplier’s current data.

Anilox line screen (lpi) Lowest BCM per in² Best BCM per in² Highest BCM per in²
120 11.10 12.60 13.50
180 6.00 7.50 9.00
250 4.70 5.80 7.00
300 4.10 4.80 5.60
360 3.60 4.30 5.00
440 2.90 3.40 4.00
550 2.60 3.00 3.50
660 1.90 2.30 2.80
800 1.50 1.80 2.10
1000 1.10 1.25 1.40
1200 0.90 0.95 1.00

Do not interpolate: for a line screen not listed, read the rows on either side and ask the supplier. Suggested line screen ranges by job type:

Job type Anilox line screen range (lpi)
Solids and coarse lines 120 to 330
Line work and text 200 to 400
Vignettes 360 to 550
Four-colour process dots 500 to 1200

The type of engraving limits the line screen. Above about 200 to 220 lpi, mechanically engraved rolls with a sprayed ceramic coating give incomplete cells. Laser-engraved ceramic reaches 1000 to 1500 lpi. A 60° cell angle works best in flexo. Small, shallow cells also need an ink with good pigment dispersion, or the pigment plugs the cells.

Anilox line screen and plate screen ruling

A common belief is that any anilox will print the highlight dots of the plate. It will not. The anilox line screen should be at least four times the plate screen ruling, and five to six times for 1 to 3% dots, so the cells are smaller than the smallest dot. The four-times rule is the most widely held view, not the only one. If a cell opening is larger than a highlight dot, the dot falls into the cell and prints dirty or heavy. The table gives the size of 1, 2 and 3% dots and the anilox line screen whose cell opening equals that dot, assuming a 5 µm cell wall.

Plate screen (lpi) 1% dot (µm) Anilox lpi, same size 2% dot (µm) Anilox lpi, same size 3% dot (µm) Anilox lpi, same size
85 34 655 48 481 58 400
100 29 754 41 557 50 464
110 26 817 37 606 45 506
120 24 878 34 654 41 547
133 22 956 31 715 37 599
150 19 1052 27 792 33 666
175 16 1187 23 901 28 760
200 14 1313 20 1004 25 851

Choose a finer anilox than the table value, so the opening is smaller than the dot:

Anilox lpi 250 300 360 400 440 500 600 660 700 800 1000 1200
Cell opening (µm) 97 80 66 59 53 46 37 33 31 27 20 16

Example. A job is screened at 120 lpi and the customer wants a 2% dot. The four-times rule alone gives at least 480 lpi. The 2% dot is 34 µm, and an anilox of 654 lpi has a cell opening of the same size. A 660 lpi anilox has a 33 µm opening, smaller than the dot, so it can keep the 2% dot on the plate. For a 110 lpi screen without small highlight dots, the four-times rule gives at least 440 lpi. The plate has to hold the same small dot; see our flexo plates.

How to check anilox volume and wear on the press

Volume falls as cells wear and plug. A simple shop check is the liquid volume method:

  1. Put a measured amount of ink on the roll, usually 25 µL.
  2. Spread it with a hand doctor blade, or roll it out with a tacky roller wrapped in a modified PE film.
  3. Transfer the ink to paper or film and measure the area of the mark in square inches.
  4. Divide µL by square inches to get BCM per square inch. For example, 25 µL over 5.0 in² is 5.0 BCM per square inch.
  5. Repeat at three positions on the roll and take the average.

“The chart numbers never match our rolls” is a common complaint. A common belief is “my own volume test should match the figure from the anilox supplier”. It will not: different measuring methods give different values, so use your own test to track change on the same roll. Keep the supplier’s figure as the baseline, plot your own readings as a wear curve for each roll, and change the roll on plan before an important job. That is how you know when the roll is worn. When readings fall, clean first; see how to clean anilox rollers. If colour is weak on a solvent-based ink, also check viscosity before you change the anilox; see the Zahn cup viscosity guide.

How to use the anilox selection chart

“Our press is different” is true for every press, so the chart is a start point, not an answer. Work in this order:

Step What to do What to check
1. Press and crew Note impression range, register, dot gain and operator skill If not assessed, the start point ignores the press
2. Job Substrate and content: solids, line, vignette or dots Coarse screens of 85 lpi or less: use the starting point table
3. Ratio rule Anilox at least four times the plate screen; five to six times for 1 to 3% dots Cell opening smaller than the smallest dot
4. Volume Read the lowest, best and highest BCM for that line screen Compare with the supplier’s current data and method
5. Engraving Laser-engraved ceramic for fine screens Ink dispersion good enough for small cells
6. Trial Run a banded test anilox (one line screen and volume per band) with a test plate Agree the result with your anilox and ink suppliers and record it

FAQ

What does BCM mean on an anilox roll?

BCM means billion cubic microns per square inch. It is the ink the cells hold per area. The metric unit is cm³/m², so check the unit on the data sheet.

Is a higher BCM anilox always better for strong colour?

No. The aim is the thinnest ink film that still gives full colour strength. Paper needs more volume than film, and solids more than dots.

What anilox line screen do I need for a 120 lpi plate?

At least four times the screen ruling, so 480 lpi. To keep a 2% dot, a 660 lpi anilox has a cell opening of 33 µm, smaller than the 34 µm dot. Confirm the choice on a trial.

What anilox volume should I use for solids?

For coarse screens, typical starting points are 220 lpi and 7.5 BCM on film, and 180 lpi and 9.5 BCM on absorbent paper. Published values differ, so the supplier’s data sheet and a trial decide.

How do I check if my anilox roll is worn?

Spread a measured amount of ink, usually 25 µL, transfer it to paper or film and divide by the area of the mark. Repeat at three positions and compare readings over time with the same method.

Why do highlight dots drop out or print dirty in flexo?

One cause is an anilox too coarse for the plate screen: the dot falls into a cell larger than itself. For 1 to 3% dots, use five to six times the plate screen.

Setting up a new flexo job? Request a quote for plates with your substrate, plate screen ruling, smallest dot and the anilox line screen and volume on your press, or ask a technical question.

Disclaimer: the line screens and volumes on this page are typical published values for reference only, not a standard’s requirement. Confirm every value with your anilox and ink suppliers and on a press trial.

About Feng Yan

Feng Yan is a technical engineer at CTPPress with more than 20 years in the printing industry and extensive front-line experience supporting printing plants. Feng specialises in solving the difficult problems printers run into in production.

Talk With Author >>

Start Your Business With Us

Simple Contact Form

Tell us what you need

Request a Quote

Tell us which printing plates or equipment you need, including specifications, quantity and destination. Use the form to send your enquiry.

Aluminium coils and printing plate production equipment
Product Enquiry

Request an Instant Quote

We reply within 24 hours on working days

Product Enquiry
Aluminium coil on an offset plate production line

Send an Enquiry


Product Enquiry
Chat on WhatsApp